Release informationCurrent Location: Home » Sell » Chemicals » Inorganic Chemicals » Oxide »

Titanium dioxide nanopowder used for textile

Click image to view full size image
Brand: Jinghe
Model: 13463-67-7
Unit price: 27.00 USD/Kilogram
MOQ: 1 Kilogram
Quantity: Negotiable
Delivery date: Since the payment date Days delivery
Share to:
Inquiry
Company Profile
 
 
Details

 

Basic information:

CAS#: 13463-67-7

Nano titanium dioxide (VK-Tvalue="25" tcsc="0" unitname="F" w:st="on">25F) can improve the comprehensive weaving performance of yarn by combining with starch and can reduce using quantity of PVA, can shortened cooking time, can lower pulp costs, can solve the problem of environmental pollution and hard to desizing of PVA slurry when it is added into textile slurry. Using Nano titanium dioxide (VK-Tvalue="25" tcsc="0" unitname="F" w:st="on">25F) instead of PVA in the yarn can play a role of posting along hairiness, filling the gap, reducing the warp breakage and lubrication.

 

Specifications:

Item no

VK-Tvalue="25" tcsc="0" unitname="F" w:st="on">25F

Appearance

White powder

pH value

6-8

Crystal type

Rutile

Particle size

30-50nm

BET, m2/g

30-50

Loss on drying value="105" tcsc="0" unitname="℃" w:st="on">105℃,2h

max 1.0%

Loss on ignition

max 2.0%

 

 

Product application:

The procedures of nano-titanium dioxide (VK-Tvalue="25" tcsc="0" unitname="F" w:st="on">25F) used in textile sizing:

1, Mixing process should maintain the original viscosity.

2, The sizing machine parameters remain stable.

3, The using amount of titanium dioxide powder: 0.5-2% by weight of starch,then gain 20% dispersion solution (A).

4, Using the same amount of starch instead of PVA, other groups were unchanged in the Cotton sizing process

5, Adding the amount of water into the mixing barrel of slurry, then shake the liquid slurry (A) of titanium dioxide additives.

7, By adding a specified amount of starch, medium speed for ten minutes and then put into other raw materials.

8, Heating and boiling slurry, then turn off the heat and keep the state of slurry for 30 minutes or 20 minutes under high pressure.

Note: 32-count yarn        using liquid (A)/barrel    value="2" tcsc="0" unitname="kg" w:st="on">2kg

     40-count yarn        using liquid (A)/barrel   value="3" tcsc="0" unitname="kg" w:st="on">3kg

     60-count yarn        using liquid (A)/barrel   value="3.5" tcsc="0" unitname="kg" w:st="on">3.5kg

If there is polyacrylate slurry in the starch formula,you should add the nano additives when the temperature of slurry is value="50" tcsc="0" unitname="℃" w:st="on">50℃.

 

Packaging: value="15" tcsc="0" unitname="kg" w:st="on">15 kg / barrel


Titanium dioxide nanopowder used for textile
 
More»Our other products
Tips:This page [Titanium dioxide nanopowder used for textile] infomation provided by [Hang zhou Wanjing New Material Co,ltd] ,the enterprise is responsible for the authenticity, accuracy and validity of the information content. Worldinout.COM do not assume any guarantee of joint and several liability. A safe way to suggest that the two sides trade, to ensure the interests of both sides.