Turbine rotor used for turbocharger and engine of ABB,GE,ALCO,EMD

YLTR-160 Superalloy tubine rotor is used for turbocharger of marine or locomotive engine

The turbocharger part is made of superalloy inconel713c

Superalloy turbine rotors are used for turbochargers,they are made of superalloy,

such as: inconel713c or inconel 718....

The turbocharger parts are used in high temperature environment, so they

have good high temperature resistance property.

Generally, turbocharger parts are used in more than 800 degrees Celsius environment

 ISO9001:2008

 

 YLTR-160

SuperalloyTurbine rotor is used for marine diesel engine spare parts

Our company's products have passed turbocharger factory's Quality Authentication,

and we also have got the ISO9001:2008 certification.

In the industry,the quality of our products is in a leading level.

Superalloy turbione wheels have a high temperature resistance property.

The turbine shaft wheel is used for turbocharger, turbojet eggine , generator etc.

The turbocharger factories give high evaluations to our turbine wheels.

Turbine wheel is a vacuum castings.

Superalloy turbine wheel, turbocharger  parts, high temperature resistant products.

 

OEM Service

We can produce all kinds of investment castings and vacuum castings. Maybe your demands of products is different from other client, please don't worry, we can produce the product according to your drawings or samples. So the product fully meet your requirements.

 

Products picture:

  

 

 

 

 

Produce best castings with heart and soul.

                                                                        ------YiLi Precision Casting

 

Turbocharger parts & turbine wheel & superalloy casting

 

Superior in quality, excellent in management,

     strong in competition, professional in manufacture.

 

WeiFang YiLi Precision Casting Co.,Ltd.

Professionally - export precision castings products.

 

Superalloy turbine wheel & turbine rotor shaft used for marine diesel engine spare parts


Superalloy turbine wheel & turbine rotor shaft used for marine diesel engine spare parts
 
More»Our other products
Tips:This page [Superalloy turbine wheel & turbine rotor shaft used for marine diesel engine spare parts] infomation provided by [Weifang Yili Precision Casting Co., Ltd.] ,the enterprise is responsible for the authenticity, accuracy and validity of the information content. Worldinout.COM do not assume any guarantee of joint and several liability. A safe way to suggest that the two sides trade, to ensure the interests of both sides.

[ Sell search ]  [ Favorites ]  [ Tell friends ]  [ Print ]  [ Close ]

 
HomeSite | About us | Contact Us | Agreement | Copyright | Sitemap | Spread | Guestbook | RSS Feed